Influence Of The Production Cycle On The Formulation And Properties Of Bodies And Glazes

Current technology for the production of porous ceramic tiles by rapid single firing is compared with traditional double firing. Changes imposed by the different processing systems on the composition of bodies and glazes are pointed out in this paper.

Author
Bruno Fabbri
Origin
Cnr Research Inst, Italy
Journal Title
Ceramic Industries International 103 1100 August 1993 12-15
Sector
Glass Ceramics
Class
GC 127

Request article (free for British Glass members)

Influence Of The Production Cycle On The Formulation And Properties Of Bodies And Glazes
Ceramic Industries International 103 1100 August 1993 12-15
GC 127