Methods, applications, advantages and disadvantages of hot and cold-crucible induction melting are discussed.
Origin
Mississippi State University, Usa
Journal Title
Am Ceram Soc Bull 83 7 2004 38-40
Sector
Special Glass
Class
S 2823