Improved Properties For Precision Moulding Phosphate Glasses

Comparisons between fluorine-free and fluorine-containing phosphate glasses as well as among three fluorine-free phosphate glasses demonstrates that a compromise between lower transition temperature and improved chemical durability can be reached through a series of composition adjustments.