An empirical model correlating thermal conductivity with volumetric bulk density and temperature for fireclay and alumina refractories has been developed.
Origin
Federal University Of Sao Carlos, Brazil
Journal Title
Am Ceram Soc Bull 81 3 2002 39-43
Sector
Refractories
Class
R 423