The feasibility of using relatively low-purity silica as the starting material for hydrothermal solidification was investigated from the consideration of effective utilization of natural resources.
Origin
Inax Corp, Japan
Journal Title
J Am Ceram Soc 84 10 2001 2318-2322
Sector
Special Glass
Class
S 2273