The surface reaction products associated with the hydrolysis of ZBLA glasses have been characterised using X-ray photoelectron spectroscopy.
Origin
Pennsylvania State University, Sandia National Laboratories
Journal Title
J Am Ceram Soc 1988 71 7 577-581
Sector
Special Glass
Class
S 156