The ground surfaces of ceramic tile are formed by brittle fracture and plastic deformation of the compositions that form combinations of craters, fracture cracks and plastic deformation grooves. Maximum glossiness and minimum surface roughness depend on the composition and microstructure of the materials and on the grinding conditions.