In-House Refractory Capability For Usa Specialist Glassmaker

Corning Inc (USA), has been making its own refractories for over 60 years. This article reviews the performance characteristics of two of its zircon refractories - ZS-835 and ZS-1324, used for the forehearths and feeder bowls in the manufacture of borosilicate and opal glasses.