Higher Production Rates Require Advanced Refractories

Increased competition in the glass industry has resulted in a demand for higher quality and productivity. The situation requires continuous improvements in all areas of the production process.

Author
K Paul
Origin
Emhart Glass
Journal Title
Glass Industry 82 3 March 2001 20-22