A high energy x-ray diffraction (HEXRD) measurement has been performed on vitreous boron trioxide (B203) at 40.9keV, using a bending magnet beamline at SPring-8.
Origin
Japan Atomic Energy Research Inst
Journal Title
Phys Chem Glasses 41 5 2000 282-285
Sector
Special Glass
Class
S 2060