The use of appropriate surfactants is an effective approach to obtain high-carbon-content castables with minimal water consumption.
Origin
University Sao Carlos, Brazil
Journal Title
Am Ceram Soc Bull 82 10/03 17
Sector
Refractories
Class
R 509