In this article, Morguerite Morrin, of IHS Chemical, analyses the global soda ash market and reports on how China has become both the largest producer and consumer of soda ash in recent years.
Origin
Ihs Chemical
Journal Title
Glass International November 2014 20-22
Sector
General
Class
G 4292