The raw materials and manufacturing technique used to produce pots at Parkinson-Spencer are reviewed. Recommendations for treatment in the glasshouse are also made.
Origin
Parkinson-Spencer Refractories Ltd
Journal Title
Glass International June 1989 35, 37
Sector
Refractories
Class
R 22