Systematic investigations on the melting behaviour and solubility of glasses of the system RO-R2O-SiO2 have been carried out to study the influence of the different oxides in certain glass systems on the HCI-resistance. The test results are correlated with field strength and the ion radius of the cation's. No regular patterns were established.