The glass transformation temperature, Tg, of an iron rich glass, made up of hazardous industrial wastes, and of the corresponding glass ceramics with different percentages of crystal phase was investigated by differential dilatometry, differential thermal analysis (DTA) and density measurements.
Origin
University Of L'Aquila, Italy
Journal Title
Glass Technology 42 4/5 2001 126-129
Sector
Glass Ceramics
Class
GC 447