An ampoule containing (formula) is placed in the furnace with the batch. The radiation is measured at various points along the furnace and in the products.
Origin
Unknown
Journal Title
Silikat Tech., 1960, 11 (12), 559-561
Sector
Primary Papers
Class
PP 664