Technological solutions available for the treatment of gaseous effluents during the production cycle of continuous glass fibre (spun glass) and of glass wool are summarised. A brief description of the final uses of the above mentioned products is given, as well as of the production cycle and marketing of the two products.
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 30 4 2000 251-256
Sector
Glass Fibre
Class
GF 262