Recent development and research trends in three important areas are discussed in this paper: a) developments in well established low thermal expansion glass ceramics; b) diverse approaches to create glass ceramics with high fracture toughenss; and c) sintered glass ceramics.
Origin
Schott Glaswerke, Germany
Journal Title
Schott Research 1996-1998 127-133
Sector
Glass Ceramics
Class
GC 373