Glass formation of a quasiternary oxide system are examined, the crystallization process and kinetics are studied and the effects of compositions, annealing conditions and oxygen deficiency on the superconductivity in the glass ceramic system are discussed.
Origin
Shanghai Institute Of Optics And Fine Mechanics, China
Journal Title
Journal Of The Australasian Ceramic Society 1991 27 1,2 57 - 75
Sector
Glass Ceramics
Class
GC 108