Direct coupling of an excimer laser to the cavity of an X-band ESR spectrometer enabled in situ observation of ultraviolet irradiation (248nm) induced effects in aluminosilicate glasses. Under these conditions the radiation was absorbed by iron traces present in the glasses and finally electron/hole pairs were formed.
Origin
Humboldt University & Fed Inst Mat Res & Testing, Berlin, Germany
Journal Title
Phys Chem Glasses 42 6 2001 401-407
Sector
Special Glass
Class
S 2326