The advantages of fusion cast refractories over bonded bricks for glass furnace regenerator packings are discussed with particular reference to Octex materials.
Origin
Toshiba Monofrax Co Ltd
Journal Title
Glass International June 1989 29, 31-32
Sector
Refractories
Class
R 21