This paper looks at some of the different Fourier transform infrared (FTIR) spectroscopic techniques that can be used to monitor the interaction of organic and inorganic coatings.
Origin
Nys College Of Ceramics, Usa
Journal Title
The Glass Researcher 9 1 1999 7-8, 16
Sector
Special Glass
Class
S 1777