Precipitation, growth and coarsening of Si3N4 crystals in liquids at 1680 deg C have been studied.
Origin
Unviersity Of Michigan, Usa
Journal Title
Jacs 86 9 2003 1578-1585
Sector
Special Glass
Class
S 2575