Ions of the transition elements have been used as optical indicators for studying the atomic structure of glass and its rearrange with heat treatment. Divalent manganese is insensitive as a colour indicator but sensitive in its characteristic fluorescence. In glasses or crystals, manganese fluoresces bright green, red, or intermediate colours.