Pilkington are now making float glass 15mm thick, compared with the previous maximum thickness of 12mm. Float glass of this new thickness now can be used for large glazed areas, subjected to extreme wind conditions. The range of thickness now available is 3-15mm; it is hoped to extend this range further in the future.