The literature on development of fibre-reinforced composites is reviewed with reference to fabrication, properties and toughening mechanisms.
Origin
Instituto De Ceramica Y Vidrio
Journal Title
Bol Soc Esp Ceram Vidr 1988 27 3 145-151
Sector
Glass Fibre
Class
GF 17