Single-edge precracked-beam (SEPB) tests were performed on a commercial lead zirconate titanate (PZT) ceramic.
Origin
Tohoku University, Japan
Journal Title
J Am Ceram Soc 85 5 2002 1243-1248
Sector
Glass Ceramics
Class
GC 459