This report forms part of a project to review and propose amendments to the benchmarks to calculate allocations to new entrants to the EU Emissions Trading Scheme (EUETS) in Phase ii (2008-2012). Enviros has been engaged by DTI to review the benchmarks for the glass sector. This report accompanies a second report that contains a review of the container and flat glass sector benchmarks also.
Origin
Unknown
Journal Title
www.Dti.Gov.Uk/Energy/Sepn/Glassrockwool_Phase2_Benchmark_Review.Pdf
Sector
Glass Fibre
Class
GF 500