The solubility and diffusion coefficients of oxygen, sulphur dioxide, and water were determined (and those for nitrogen, carbon dioxide, and argon were estimated) in commercial E-glass melts as a function of melt temperature and atmosphere.
Origin
Virginia Military Institute
Journal Title
J Am Ceram Soc 1989 72 9 1680-1691
Sector
Glass Fibre
Class
GF 43