Epr And Magnetic Susceptibility Studies On Mn0-B203-Cd0 Glasses

Electron paramagnetic resonance (EPR) of Mn2+ ions revealed their distribution on different structural units of 2B203, Cd0 glass matrix doped with Mn0. Distorted octahedral symmetric sites were detected. The progressive clustering of Mn2+ ions was evidenced when the Mn0 content increased.