Chromium oxide (Cr203) solubility was measured in soda lime borosilicate glass from 1400 to 1500K. The temperature dependence of the solubility increased with increased sodium oxide concentration. The ethalpies of solution for the equilibrium phases were calculated from the solubility data in the temperature range from 1400 to 1500K.
Origin
Korea Hydro & Nuclear Power Co, Yusung
Journal Title
J Am Ceram Soc 84 12 2001 2987-2990
Sector
Special Glass
Class
S 2298