Research sponsored by the Thermal Insulation Manufacturers Association on determining the effects of mineral fibres on health and various in-house projects by American fibre manufacturers are reviewed. Methods of enginering controls are discussed.
Origin
Unknown
Journal Title
Ceramic Bulletin 1989 68 12 2092-2097
Sector
Glass Fibre
Class
GF 52