Successful field trials in commercial slagging gasifier systems have been made of improved refractory materials engineered specifically for longer service life in this application.

Author
K Kwong Et Al
Origin
Albany Research Centre, Usa
Journal Title
Am Ceram Soc Bull 85 2 2006 17-20
Sector
Refractories
Class
R 620