Two alginate (Alg) based coatings on stainless steel AlSl316L substrates, one containing titania nanoparticles and another one a mixture (50/50wt-%) of n-TiO2 and bioactive glass (BG), intended for biomedical applications, were developed by electrophoretic deposition (EPD) from ethanol/water suspensions. Different n-TiO2 (2-10gL-1) and BG (1-5gL-1) contents were studied for a fixed alginate concentration and the properties of the electrophoretically obtained coatings were characterised.