The results of a questionnaire completed by Japanese technologists were used to help predict future R&D trends for dielectric ceramics, piezoelectric ceramics and ferroelectric thin films.
Origin
Nextech Materials Ltd, Usa
Journal Title
Am Ceram Soc Bull 76 8 1997 51-55
Sector
Glass Ceramics
Class
GC 287