New glasses in the system xAgI.(1-x)[Ag20:Te02] were prepared and investigated. The glass forming region in the system is identified by x-ray diffraction. The amorphous nature of glasses of 60 mol%). Some physical properties of glasses in the above given system have been studied.
Origin
Mansoura University, Egypt
Journal Title
Phys Chem Glasses 41 1 2000 6-9
Sector
Special Glass
Class
S 1879