This article discusses an investigation into the development in chemical composition and the size of the bubbles occurring in the glass melt. The bubble trajectories were investigated in an electric melter with new top electrodes, as well as in a furnace with 40% electrode corrosion.
Origin
Institute Of Glass & Ceramics, Czech Republic
Journal Title
Glass International June 2010 26-28 30-31
Sector
Special Glass
Class
S 3586