Effects Of Phse Separation And Devitrification Processes In Oxide Glasses On Esr Spectra

The consequences of phase separation and devitrification processes for the ESR patterns of Fe3+ ions and oxygen hold centres in glassy and glassy-crystalline systems are discussed. analysis of the Fe3+ spectra by simulation (including 4th order terms) allows their model-based interpretation for homogeneous, phase-separated and devitrified samples as well. It is even possible to estimate the ratio of Fe3+ ions incorporated into the glassy matrix to those localized in the crystalline phase.

Author
M Nofz Et Al
Origin
Bundesanstalt Fur Materialforschung Und-Prufung, Berlin
Journal Title
Glastech Ber Glass Sci Technol 70 9 1997 272-277
Sector
Special Glass
Class
S 1261

Request article (free for British Glass members)

Effects Of Phse Separation And Devitrification Processes In Oxide Glasses On Esr Spectra
Glastech Ber Glass Sci Technol 70 9 1997 272-277
S 1261
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.