In this study, Li20-TiO2-P205-x(Fe203) (x=0, 2.5, 5 and 7.5 weight part) glass and glass-ceramics were synthesized through conventional melt-quenching method and subsequently heat treatment. Glass samples were studied by UV-visible spectroscopy and crystallized samples were characterized by differential thermal analysis, X-ray diffractometry and field emission scanning electron microscopy. Besides, electrical properties were examined according to the electrochemical impedance spectroscopy techniques.
Origin
Sharif University Technology, Iran
Journal Title
Materials Chemistry & Physics 190 2017 8-16
Sector
Glass Ceramics
Class
GC 888