Glass fibres were drawn from three MgO-Al203-Y203-Si02-based oxynitride glass melts. a single-hole bushing process was used to spin the melts containing nitrogen between about 13 and 16 at.%. The drawing process is described in detail, and it is shown that besides melt viscosity the high surface tension of the oxynitride glass melts strongly controls the fiberization. This is analyzed in terms of Reynolds and Weber numbers.
Origin
Inst Fur Nichmetallische & Tech Univ Clausthal, Germany
Journal Title
Glastech Ber Glass Sci Technol 70 4 1997 109-112
Sector
Glass Fibre
Class
GF 179