Solutions of pure sand and glass were made with the aid of Eppendorf micro-test tubes in order to overcome the problem of reagent impurity in trace analyses.
Origin
Unknown
Journal Title
Analytical Chemistry 46 7 1974 965-966
Sector
Primary Papers
Class
PP 1200