The dissolution behaviour of two types of fibres, the biosoluble HT and the traditional MMVF21 stone wool fibres, in synthetic simulated lung fluid (Gamble's solution) at pH4.5 was investigated in order to clarify the mechanisms, and the effect of the various constituents in the liquid.