Development Of Oxygen-Fuel Combustion For Glass Melting

Several economic, environmental and national energy realities shaping world policies are reviewed to demonstrate the benefit of departing from conventional regenerative glass melting to direct-fired oxygen-fuel combustion for glass melting.

Author
J T Brown
Origin
Corning Inc
Journal Title
Glass Production Technology International 1992 71-73