A method is described for the determination of impurities such as iron, chromium, manganese, nickel, cobalt and copper in the glass raw materials limestone and dolomite. The proposed method involves the direct measurement technique in aqueous solution by flame atomic absorption spectrometry. It has been proved to be an accurate and quick method for analyzing concentrations normally found in these raw materials.
Origin
Turkiye Sise Research Centre & Stazione Sperimentale Del Vetro
Journal Title
Glastech Ber Glass Sci Technol 70 10 1997 289-297
Sector
Special Glass
Class
S 1376