The properties of glass-ceramics depend upon composition and microstructure. These are reviewed along with novel and recent applications for glass-ceramics.
Origin
Corning Glass Works
Journal Title
Ceramic Technology International 1992 89 - 93
Sector
Glass Ceramics
Class
GC 112