Barium iron phosphate glasses were investigated with DSC analysis and infrared spectroscopy to study the effect of the increasing concentration of Fe203 in (50-x) Ba0.XFe203.50P205 glasses and to explain the structure-property relationships in this system.
Origin
Lpcs, Morocco
Journal Title
Phys Chem Glasses 43 3 2002 129-132
Sector
Special Glass
Class
S 2601