The density and molar volume of Li20-Si02 glasses have been analysed for glasses containing up to 64 mol% Li20. The analyses are based on a model that makes use of the fractions of the structural units present in glass.
Origin
Mansoura University, Egypt
Journal Title
Phys Chem Glasses 39 5 1998 286-289
Sector
Special Glass
Class
S 1564