The features occurring in soda-lime-silica and silica glasses beneath pyramidal indenters with included angles of 125, 136 and 150 degrees have been explored by the traditional process of sectioning the indenters.
Origin
University Of Keele
Journal Title
Glass Technology 1990 31 3 121-125