KIWO introduced a range of resists for glass applications at the glasstec exhibition in 2012. Using a resist, the glass surface can be masked by design, either partially or full-faced, prior to further finishing, processing or transport, thus being protected from outside influences. Applications such as etching, sandblasting or sputtering are the focal point of this range. The resists are medium to highly viscous emulsions. Depending on product and screen printing task, application is by spraying, rolling (roller coating) or dipping.