In order to develop phlogopite based machinable glass ceramics with optimum properties, the influence of their crystallisation characteristics was investigated by varying the content of nucleating agent, temperature of heat treatment and forming methods. The effect of these factors on the utility of these glass ceramics was discussed.
Origin
Wuhan University, China
Journal Title
Glass Technology 37 5 1996 175-178
Sector
Glass Ceramics
Class
GC 253